Search Jensen
Authentic® Shoulder Porcelain Technique Guide

SHADE
SHOULDER PORCELAIN
RATIO
A1
M2+ M1
3 to 1
A2
M2
100%
A3
M3+ M5
2 to 1
A3.5
M4+ M5
1 to 1
A4
M4 +M5
2 to 1
B1
M1+ M2
4 to 1
B2
M1+ M2
2 to 1
B3
M3
100%
B4
M4+ M3
3 to 1
C1
M2 +M6
1 to 1
C2
M6 +M2
2 to 1
C3
M6+ M5
3 to 1
C4
M6+ M5
4 to 1
D2
M2 +M5
4 to 1
D3
M2+ M5+ M6
3 to 2 to 1
D4
M2+ M5
3 to 1

 

Authentic® Shoulder Porcelain Technique Guide
Firing Guide
 
Close
Time
Start
Temp
First
Firing
Second
Firing
Rate of
Climb
Start
Vacuum
Hold
Time
Shoulder
Porcelain
4 min
400º C
770º C
760º C
45º / min
450º C
1 min